Revishield® 71T8-Ni2

General description

Self shielding: easiest equipment

Higher strength level, yield strength up to 450 N/mm

Excellent impact toughness at -40°C

CTOD tested, offshore constructions

Current type / Shielding gases

DC -

Approvals

ABS

GL

LR

3SA, 3YSAН10

3YSH10

3S, 3YSH10

Suggestions for use

Off-shore oil equipment, piping, storage tanks

General plate fabrication including bridge construction on ships and barges

Circumferential groove welds for heavy wall, large diameter tubular construction

Classification

AWS A5.29/A5.29M

:E71Т8-Ni2 (also meets: E81T8-Ni2)

Welding positions

               

Typical chemical composition of all weld metal, (w%)

C

Mn

Si

P

S

Al

Ni

0.07

0.26

0.06

0.004

0.002

0.88

2.44

Mechanical properties of all weld metal

 

Shieldin gas

Condition

Yield strength (N/mm2)

Tensile strength (N/mm2)

Elongation (%)

Impact (ISO), J

+20oС

-29oС

-40oС

Required

AWS A5.29

 

 

min 400

480-620

20

 

27

 

Typical values after welding

 

AW

500

570

28

 

88

84