All position gas shielded 1% Ni flux cored wire, offshore and similar applications
Specific design for stress relieved applications, guaranteed impact properties after PWHT
Superior weldability, low spatter, good bead appearance
Outstanding operators appeal
Exceptional mechanical properties (CVN >47J at -40°C)
Very low hydrogen HDM <5 ml/100g
Superior product consistency with optimal alloy control
Very good wire feeding
DC +
Ar+(>5-25%) CO2 (EN 439: M21)
15-25 l/min
|
Shielding gases |
BV |
DNV |
GL |
LR |
|
М21 |
4YSDH5 |
IVYMSН5 |
4YH5S |
4YSH5 |
|
Unit type |
Net weight/unit (kg) |
Diameter (mm) 1.2 |
1.6 |
|
Plastic spool S200 |
4.5 |
Х |
|
|
Wire reel B300 |
15 |
Х |
Х |
|
Wire reel В435 |
25 |
X |
|
|
AWS A5.29/А5.29М |
:E81T1-Ni1M- JH4 |
|
EN 758 |
:T 50 5 1 Ni P M 2 H5 |

|
Shielding gases |
C |
Mn |
Si |
P |
S |
Ni |
|
HDM ml/100g |
|
М21 |
0.06 |
1.4 |
0.3 |
0.013 |
0.010 |
0.95 |
|
3 |
|
|
Shielding gas |
Condition |
Yield strength (N/mm2) |
Tensile strength (N/mm2) |
Elongation (%) |
Impact (ISO), J |
||
|
-40oС |
-50oС |
|||||||
|
Required |
AWS A5.29 |
|
|
min.470 |
550-690 |
min. 19 |
min. 27 |
|
|
EN 758 |
|
|
min.500 |
560-720 |
min. 18 |
|
min.47 |
|
|
Typical values after welding |
M21 |
AW |
570 |
620 |
24 |
120 |
100 |
|
|
M21 |
SR |
550 |
600 |
24 |
120 |
100 |
||
| Revicod® 81T1-A1M |
| Revicod® 101T1 |
| Revicod® 81T1-K2M |
| Revicod® 81T1-Ni1M |