Electrode for welding of rolled and cast martensitic steel. Gives martensitic structure of metal weld. During welding of thick plates it is recommended to heat up to 100-120оС with further heat treatment for retained stress relieving – 650оС. Covering type – rutile-basic.
DC (+)
Electrodes after removal from packing redry 2-4h 350 ± 25оС
|
AWS A5.4 |
:E410 NiMo - 16 |
|
EN 1600 |
:E 13 4 R 3 2 |

|
UNS |
Alloy |
EN/ Symbol Material N° |
|
J91540 |
CA6-NM |
G-X5CrNi 13-4 1.4313 |
|
S41500 |
|
X3CrNiMo 13-4 1.4313 |
|
|
|
G-X4CrNi 13-4 1.4317 |
|
|
|
G-X5CrNiMo 13-4 1.4407 |
|
|
|
X3CrNiMo 13-4 1.4413 |
|
|
|
G-X4CrNiMo13-4 1.4414 |
|
C |
Mn |
Ni |
Si |
Cr |
Mo |
Cu |
|
0.03 |
0.7 |
4.6 |
0.50 |
12.0 |
0.50 |
<0.3 |
|
|
Condition |
0,2% yield strength (N/mm2) |
Tensile strength (N/mm2) |
Elongation (%) |
Impact (ISO), J |
|
Typical values after welding |
AW |
650 |
870 |
17 |
45 |